Wednesday, October 7, 2009

Making Madder Lake - Part 3

It has been three days since the alum was added, and the frothing has died down. The next step is to pour the liquid into a larger bucket and to fill the remainder of the larger bucket with cold water:




Now, this mixture will sit for 36 hours to allow the sediment to settle to the bottom of the bucket. Then, I will begin the process of siphoning water from the bucket until it comes out clear, which will be covered in my next post.

For those who are bored by all of this technical detail, hang tight -- we will be back to the violin soon.

Sunday, October 4, 2009

Making Madder Lake - Part 2

The madder root/potash solution has now been heated for 36 hours at a low temperature of 40 to 45 degrees celsius:


The next step is to filter out the madder root and sediment so that a red liquid remains. To do that, I am using a fine cotton cloth taped inside a bucket with a strainer over it and mesh cloth in the strainer (whew!) . Here are the component parts and the assembly:



The mesh in the strainer is intended to catch the large particles so that they don't clog up the finer filter in the cotton cloth. Here it is in action:


I had to replace the cotton cloth a few times because it was getting clogged -- this could probably be avoided by using whole madder root instead of ground madder root, but I used ground root because Kremer was out of stock of whole root. After straining, red liquid is left at the bottom of the bucket (although the deep red color of the liquid doesn't show well in these pictures):


Next, a solution of warm water and alum is prepared and added to the bucket:



As you can see, adding the alum solution causes a lot of frothing and creates a muddy mixture:


This muddy mix needs to sit for three days and stirred once or twice per day. At that point, the frothing will die down and it will be ready for the next steps. Expect an update post mid-week.

Friday, October 2, 2009

Making Madder Lake - Part 1

Before beginning the varnish process, I am taking time to make some madder lake pigment. For readers who aren't violinmakers, madder lake is a red pigment made from the roots of a madder plant and is often used for the red color on violins. This pigment will, if I am successful, be used to add the red color to the varnish on my violin. There is, of course, plenty of madder lake around the studio that I could use, but I wanted the experience of making my own. I will be following the instructions for making madder lake from the late David Rubio's website (www.rubioviolins.com). The process will take a week or two, so I will post updates as the process moves along. Hopefully the end result will be a useable pigment.

The first step is to combine the madder root with potash in water and heat the mixture at 40-45 degrees celsius for 36 hours.

Here are the measured madder root and potash:


The ingredients are then added to the heated water:


It is important to maintain the low temperature to maintain the red color, so I will check temperature and stir the mixture regularly over the next 36 hours:


The next post on Sunday will show the next steps after the heating is complete. Cross your fingers and wish me luck!

Monday, September 28, 2009

Out of the UV Box

After a little more than a week of tanning in the UV lights, the parts of my violin have a darker appearance (although it is difficult to show the exact color changes in quick photos taken on a dreary day):


Thursday, September 17, 2009

UV Light Tanning

I have spent time cleaning up various surfaces and lines with Gregg’s help to prepare the parts of the violin for UV tanning and then for varnishing. Here are the finished parts of the violin "in the white":

After the parts of the instrument cleaned up, they are placed into the UV light box for tanning:

The parts will remain in the UV light box for about a week and will then emerge with a much darker appearance.

Tuesday, September 8, 2009

Trimming the Bass Bar

Now that the bass bar has been fitted and glued into place, the top contour of the bar is shaped with a small plane:

I measure frequently while trimming until I reach my desired heights -- 12.5mm in the center of the bar tapering to 4.5mm at the ends of the bar:

When the desired measurements are achieved, the sides of the bar are beveled/rounded:

Then, a bevel and tab is cut on each end of the bar with a shallow gouge – the tab ends 40mm from the edge of the plate, and the bevel begins 45mm from the edge of the plate:

Here is the finished bass bar:

Next, I have some cleanup work to do on the parts before the varnishing process begins.

Tuesday, September 1, 2009

Fitting the Bass Bar

One of the most challenging tasks that I have faced thus far in my apprenticeship is properly fitting a bass bar. As a prerequisite to fitting the bar, the interior surface of the top plate must be finished well – smooth arch, no bumps or irregularities.

The bass bar starts as a stick of spruce that is 5.5mm thick. The exact placement of the bass bar is then calculated and pencil lines are made in the appropriate places. Although many makers use wooden studs to assist them in fitting the bassbar, I am using the Alf Studios bass bar frame, as pictured below. The edges of the top plate are clamped to the frame to minimize distortion, and the arms of the bass bar frame are adjusted so that the rough bass bar stock is aligned with the pencil lines and thus in the proper place:

The rough bass bar stock is then placed into an acrylic jig and roughly trimmed to the appropriate curve:

Then, chalk is used to fit the bar exactly to the inside curve of the top plate. First, powdered chalk is brushed onto the inside of the top plate. When brushing the chalk, it is important to try to attain an even distribution of chalk dust throughout the surface where the bass bar will touch:

When the chalk is evenly distributed, the bar is lowered carefully into position and rubbed slightly from side to side:

The bar is then removed, and the chalk marks on the bottom of the bar indicate where the bar is making contact with the top plate. If the entire bottom surface of the bar isn’t covered with chalk, then the chalk marked high spots are removed with a small plane, and the process is repeated until the fit is perfect in all dimensions. The process for me entailed hours of doing this:

To make matters a bit more complicated, the bass bar in my violin is “sprung,” which means that the ends of the bar rise from the surface of the plate by .5mm and are later pressed flush with the surface when glued and clamped. This requires a perfect fit in the middle of the bar and .5mm gaps at the ends of the bar, such that the end gaps close when the bar is rocked to either side or when light pressure is applies at both ends of the bar.

Once a perfect fit is achieved, which is much more difficult to do than it may sound, the bar is clamped and glued into place as follows:

When the glue dries, the clamps are removed and the top contour of the bass bar is trimmed, which will be the subject of my next blog entry.